PHPA is a high molecular weight polymer with a moderate anionic charge for drilling mud additive. It can be used in both industrial and oil field drilling application and it is usable in both fresh water and brines. It can be used in high temperature.Applications: 1) Shale stabilization2) Viscosifier3) Friction reduction4) Fluid loss control5) LubricationSpecifications: 1) Appearance: off white powder2) Degree of charge: 15 - 45%3) Molecular weight: 5 - 204) Solid content: 89% min.To obtain homogeneous solution, efficient dispersion is necessary. The most convenient method of dispersing these products is with a polymer eductor or a commercially available dry powder feeder unit. Solution should be made up at 0.1 - 0.3% solid. Make-up water temperature should be between 10 and 40°C for optimum product performance. Following dispersion into agitated water, stirring should continue for about an hour to ensure complete dissolution. Stirring maybe carried out by propeller type stirrer with a speed of 200 - 500rpm. It is recommended to have both a stock make-up tank and a solution holding tank for dosage into the system. The above recommended anionic solution concentration are stable for up to one week. Aluminum, zinc, copper, or iron should be avoided in make-up system.Packing: 25kg/compounded or multi-wall bag or according to customers' requirements